Morphology and crystal structure
Grey black powder, Without aggregation.
Use suggestion
This product can be used as a cathode material in the manufacture of lithium ion secondary batteries.
The full battery design capacity of this product with graphite negative electrode: 153mAh / g (0.5C, 4.2V-3.0V) (affected by the customer's process, the data has a certain degree of fluctuation)
It is recommended to bake the material at 120 ºC for 6h before mixing.
Processing design compaction 3.20 ~ 3.40g / cm3 (Affected by the customer's process, the data has a certain degree of fluctuation).
According to the performance requirements, choose an appropriate electrolyte that matches the nickel-cobalt manganese oxide.
Chemical index
Project | Unit | Standard | Reference | The analytical methods |
Li | % | 7.0~8 | 7.1 | ICP |
Ni+Co+Mn | % | 57~62 | 59.2 | ICP |
Ca | % | ≤0.0200 | 0.0035 | ICP |
Cu | % | ≤0.0050 | 0.0002 | ICP |
Fe | % | ≤0.0010 | 0.0003 | ICP |
Na | % | ≤0.0300 | 0.0188 | ICP |